Clinker Type 2
Clinker, in the production of Portland cement, are the heat treated beams, typically 3 to 25 mm diameter. They are creating by heating limestone and aluminum silicate (clay) during the cement furnace stage. Clinker-the raw material for cement production-is a processed product which is using in cement composition, based on the cement type.
Data Sheet
| DAILY QUALITY CERTIFICATE | Composition | ISIRI 389 | ASTM C150 | EN 197-1 | %Mass Fraction | |
| Loss on Ignition | % | LOI | Max 3.0 | Max 3.0 | – | 0.19 |
| Silicon Dioxide | % | SiO2 | Min 20.0 | Min 20.0 | – | 21.94 |
| Aluminium Oxide | % | Al₂O₃ | Max 6.0 | Max 6.0 | – | 5.79 |
| Ferric Oxide | % | Fe2O3 | Max 6.0 | Max 6.0 | – | 4.43 |
| Calcium Oxide | % | CaO | – | – | – | 64.16 |
| Magnesium Oxide | % | MgO | Max 5.00 | Max 6.00 | – | 2.26 |
| Sulfur Trioxide | % | SO3 | Max 3.0 | Max 3.0 | – | 0.39 |
| Sodium Oxide | % | Na2O | – | – | – | 0.2 |
| Potassium Oxide | % | K2O | – | – | – | 0.62 |
| Chlorides | % | Cl | – | – | – | 0.01 |
| TOTAL | Total | – | – | – | 99.99 | |
| Insoluble Residue | % | IR | Max 0.75 | Max 1.5 | – | 0.22 |
| Free CaO | % | F.CaO | – | – | – | 0.66 |
| Lime Saturation Factor | % | LSF | – | – | – | 90.18 |
| Silica ration | % | SIM | – | – | – | 2.15 |
| Alumina ratio | % | ALM | – | – | – | 1.31 |
| Tricalcium Silicate | % | C3S | – | – | – | 48.04 |
| Dicalcium Silicate | % | C2S | – | – | – | 26.68 |
| Tricalcium Aluminate | % | C3A | Max 8.00 | Max 8.00 | – | 7.85 |
| Calcium Alumino Ferrite | % | C4AF | – | – | – | 13.47 |
| C3A + C3S | % | – | – | – | – | 55.89 |
| C4AF + 2C3A | % | – | – | – | – | 29.16 |
| Alkalies (Na2O+ 0.658 K2O) | % | – | – | – | – | 0.61 |


Packaging
- Bulk
Transportation
- Land
- Rail
- Sea
Application
- Produce moderate heat cement