Clinker Type 5
Clinker, in the production of Portland cement, are the heat treated beams, typically 3 to 25 mm diameter. They are creating by heating limestone and aluminum silicate (clay) during the cement furnace stage. Clinker-the raw material for cement production-is a processed product which is using in cement composition, based on the cement type
Data Sheet
Daily Quality Certificate | Composition | ISIRI 389 | ASTM C150 | EN 197-1 | %Mass Fraction | |
Loss on Ignition | % | LOI | Max 3.0 | Max 3.0 | Max 5.0 | 0.25 |
Silicon Dioxide | % | SiO2 | – | – | – | 21.8 |
Aluminium Oxide | % | Al₂O₃ | – | – | – | 4.66 |
Ferric Oxide | % | Fe2O3 | – | – | – | 5.07 |
Calcium Oxide | % | CaO | – | – | – | 65.11 |
Magnesium Oxide | % | MgO | Max 5.00 | Max 6.00 | – | 1.89 |
Sulfur Trioxide | % | SO3 | Max 2.3 | Max 2.3 | Max 3.0 | 0.39 |
Sodium Oxide | % | Na2O | – | – | – | 0.17 |
Potassium Oxide | % | K2O | – | – | – | 0.61 |
Chlorides | % | Cl | – | – | – | 0.01 |
TOTAL | Total | – | – | – | 99.96 | |
Insoluble Residue | % | IR | Max 0.75 | Max 1.5 | Max 5.0 | 0.21 |
Free CaO | % | F.CaO | – | – | – | 0.86 |
Lime Saturation Factor | % | LSF | – | – | – | 93.23 |
Silica ration | % | SIM | – | – | – | 2.24 |
Alumina ratio | % | ALM | – | – | – | 0.92 |
Tricalcium Silicate | % | C3S | – | – | – | 59.65 |
Dicalcium Silicate | % | C2S | – | – | – | 17.52 |
Tricalcium Aluminate | % | C3A | Max 5.00 | Max 5.00 | Max 5.0 | 3.77 |
Calcium Alumino Ferrite | % | C4AF | – | – | – | 15.41 |
C3A + C3S | % | – | – | – | – | 63.42 |
C4AF + 2C3A | % | – | Max 25.0 | Max 25.0 | – | 22.95 |
Alkalies (Na2O+ 0.658 K2O) | % | – | – | – | – | 0.57 |
Packaging
- Bulk
Transportation
- Land
- Rail
- Sea
Application
- Make the sulphate resistance OPC